Charlie,
Well, you ain't gonna like my answer. Try one coat and sand with 150. Or better yet do a coat and sand with a fairing board. You'll have to level the highs and fill the lows as you go. Once you get even results with the fairing board, you could carry on with 220 grit on the ROS.
Please take the time now - you'll thank yourself later.
Zen of sanding.
In Response to: 80-grit sanding by Charlie Walsh on May 25, 2004
Replies:
- Re: 80-grit sanding by Peter Lyons on May 25, 2004
-
Re: 80-grit sanding by Charlie Walsh on May 26, 2004
- Re: 80-grit sanding by Kurt Maurer on May 26, 2004
- Re: 80-grit sanding by Mac on May 26, 2004
- Re: 80-grit sanding by Steve Miller on May 26, 2004
- Re: 80-grit sanding by Kurt Maurer on May 26, 2004
- Re: 80-grit sanding by RogerJ on May 26, 2004
- Re: 80-grit sanding by Mark Camp on May 26, 2004
- Re: 80-grit sanding by Kurt Maurer on May 26, 2004
- Re: 80-grit sanding by Steve Miller on May 26, 2004
- Re: 80-grit sanding by Joe Lombardo on May 26, 2004
- Re: 80-grit sanding by RogerJ on May 26, 2004
- True Confessions by Kurt Maurer on May 26, 2004
- Re: Fairing Board by Dave Houser on May 26, 2004
- Re: True Confessions by Peter Lyons on May 26, 2004
- True Confessions by Kurt Maurer on May 26, 2004
- Re: 80-grit sanding by RogerJ on May 26, 2004
-
Re: 80-grit sanding by Charlie Walsh on May 26, 2004